MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Dyneon™ PFE 4131TZ High Temperature Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dyneon™ PFE 4131TZ is an incorporated cure high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per ASTM D1418. Its fully fluorinated back bone structure provides a very broad chemical and thermal stability.
    Features and Benefits:
  • Incorporated cure version of PFE 131TZ
  • Ideal for dry side (thermal processes) semiconductor applications including plasma, and high temperature CPI and aerospace applications
  • High temperature FFKM
  • Low metal ion content with low extractables
  • Upper use temperature of 315°C
  • Excellent compression set resistance
  • Can be compounded to pass AMS 7257

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.00 g/cc2.00 g/cc
Mooney Viscosity 100
@Temperature 121 °C
100
@Temperature 250 °F
ML 1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8181Press cure 15 Minutes @ 188°C, Post Cure 16 Hours @ 250°C
Tensile Strength at Break 17.1 MPa2480 psiPress cure 15 Minutes @ 188°C, Post Cure 16 Hours @ 250°C
Elongation at Break 155 %155 %Press cure 15 Minutes @ 188°C, Post Cure 16 Hours @ 250°C
100% Modulus 12.1 MPa
@Strain 100 %
1750 psi
@Strain 100 %
Press cure 15 Minutes @ 188°C, Post Cure 16 Hours @ 250°C
Compression Set  17 %
@Treatment Temp. 232 °C,
Time 252000 sec
17 %
@Treatment Temp. 450 °F,
Time 70.0 hour
Method B, -214 O-rings, Aged 70 Hours, 25% Deformation; ASTM D395
 33 %
@Treatment Temp. 232 °C,
Time 605000 sec
33 %
@Treatment Temp. 450 °F,
Time 168 hour
Method B, -214 O-rings, Aged 168 Hours, 25% Deformation; ASTM D395
 39 %
@Treatment Temp. 300 °C,
Time 252000 sec
39 %
@Treatment Temp. 572 °F,
Time 70.0 hour
Method B, -214 O-rings, Aged 70 Hours, 18% Deformation; ASTM D395
 46 %
@Treatment Temp. 300 °C,
Time 605000 sec
46 %
@Treatment Temp. 572 °F,
Time 168 hour
Method B, -214 O-rings, Aged 168 Hours, 18% Deformation; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 315 °C599 °F
Brittleness Temperature -35.0 °C-31.0 °F
Transformation Temperature -2.00 °C28.4 °FTR10
 
Descriptive Properties
ColorOff-White
FormSlab
MH, Maximum Toque17.6 inch-lb100 cpm, 0.5° Arc, 12 Minutes @ 188°C
ML, Minimum Torque0.95 inch-lb100 cpm, 0.5° Arc, 12 Minutes @ 188°C
t2, Time to 2 Inch-lb Rise from Minimum1.7 Minute100 cpm, 0.5° Arc, 12 Minutes @ 188°C
t'50, Time to 50% Cure2.9 Minutes100 cpm, 0.5° Arc, 12 Minutes @ 188°C
t'90, Time to 90% Cure6.0 Minutes100 cpm, 0.5° Arc, 12 Minutes @ 188°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ 2299X Ultra High Viscosity Fluoroelastomer
3M Dyneon™ 81T High Temperature Perfluoroelastomer
3M Dyneon™ PFE 60 Perfluoroelastomer
3M Dyneon™ TFE 90 Peroxide Cure Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 8475 FFKM Perfluoroelastomer

PDYL9972 / 129990

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.