MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestoran® X4890 sw PPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Molded

Material Notes: Impact resistant PPE resin with a heat deflection temperature of 125°C. VESTORAN X4890 has a very good flow properties and a high impact resistance. Parts with large surfaces exhibit a regular matte surface finish.

Applications: Housing parts, automotive industry, electroindustry, environmental technology.

ISO data as provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³
Water Absorption 0.00 %0.00 %
Melt Flow 96 g/10 min96 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.0 MPa5800 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 3.0 %3.0 %
Modulus of Elasticity 2.00 GPa290 ksi
Charpy Impact Unnotched NBNB
Charpy Impact, Notched 3.30 J/cm²15.7 ft-lb/in²
Tensile Impact Strength 268 kJ/m²128 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 3.00e+14 ohm3.00e+14 ohm
Dielectric Constant  2.0
@Frequency 100 Hz
2.0
@Frequency 100 Hz
 2.0
@Frequency 1e+6 Hz
2.0
@Frequency 1e+6 Hz
Dielectric Strength 29.0 kV/mm737 kV/in
Dissipation Factor  0.00010
@Frequency 100 Hz
0.00010
@Frequency 100 Hz
 0.00080
@Frequency 1e+6 Hz
0.00080
@Frequency 1e+6 Hz
Comparative Tracking Index 200 V200 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 125 °C257 °F
Deflection Temperature at 1.8 MPa (264 psi) 107 °C225 °F
Vicat Softening Point 130 °C266 °F50°C/hr/50 N

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestoran® X4893 sw PPE
Evonik Vestoran® 1900 GF20 20% Glass Reinforced PPE Compound
Vestolit® Pulver 4101 PVC-U
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer
Solvay FM® 6555-1 Ester Syntactic Core

PHUM58 / 47491

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.