MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS Tristar® PC-30GFR 30% Glass Reinforced Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 30% Glass Filled

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D792
Water Absorption 0.12 %0.12 %24 hrs; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 128 MPa
@Thickness 3.17 mm
18500 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 3.0 %
@Thickness 3.17 mm
3.0 %
@Thickness 0.125 in
ASTM D638
Flexural Strength 155 MPa
@Thickness 3.17 mm
22500 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 7.58 GPa
@Thickness 3.17 mm
1100 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secPLC 6
Comparative Tracking Index 100 - 175 V100 - 175 VPLC 4
Hot Wire Ignition, HWI 60 - 120 sec60 - 120 secPLC 1
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsPLC 0
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 143 °C290 °FASTM D648
UL RTI, Electrical 80.0 °C176 °F
UL RTI, Mechanical with Impact 80.0 °C176 °F
UL RTI, Mechanical without Impact 80.0 °C176 °F
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate
Aclo Accutech Polycarbonate POL050G30L Glass Reinforced
Overview of materials for Polycarbonate, 30% Glass Filled
PTS Tristar® PC-30GF 30% Glass Reinforced Polycarbonate With Release
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced

PZ9PU20e / 79037

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.