MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Absolac® XT04PM Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Absolac XT04(PM) is high heat grade suitable for injection molding applications. high heat grade, good impact strength. Applications: automotive parts, lamp housing, automotive interior parts, microwave oven housings.

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
Melt Flow 5.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
5.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ISO 2039-2
Tensile Strength, Yield 55.0 MPa7980 psiISO 527
Tensile Modulus 2.80 GPa406 ksiISO 527
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 2.80 GPa406 ksiISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
0.25 inch bar, 0.01 notch radius; ISO 180/A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 100 µm/m-°C38.9 - 55.6 µin/in-°FISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 103 °C217 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 110 °C
@Load 5.10 kg
230 °F
@Load 11.2 lb
B/2 120C/H; ASTM D 1525
 
Optical PropertiesMetricEnglishComments
Gloss 98 %98 %at 60°, specular; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bhansali Engineering Abstron IM17A TT ABS Injection Molding Grade
Bhansali Engineering Abstron IM17V ABS Injection Molding Grade

PSTYR9806 / 216033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.