MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excellent sealing material with a very low seal initiation temperature and high clarity.

Availability: Latin America, North America and South America

Applications:

  • Adhesive Lamination
  • Barrier Food Packaging
  • Coextrusion Coating
  • Compounding
  • Document Plastification
  • Extrusion Coating
  • Extrusion Lamination
  • Flexible Packaging
  • High Frequency Sealing
  • Industrial Packaging
  • Injection Molding
  • Masterbatch Base Resin
  • Non-woven Coating
  • PVC Replacement
  • Thermal Lamination
  • Wire and Cable Compounds

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³ExxonMobil method
Vinyl Acetate Content 18 %18 %ExxonMobil method
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 190 °C
14 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In  9.40 cm
@Temperature 230 °C
3.70 in
@Temperature 446 °F
656 ft/min, constant output at 35 rpm; ExxonMobil Method
 10.9 cm
@Temperature 230 °C
4.30 in
@Temperature 446 °F
328 ft/min, constant output at 35 rpm; ExxonMobil Method
Drawdown 9.00 m/s
@Temperature 230 °C
1770 ft/min
@Temperature 446 °F
Constant output at 35 rpm; ExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 90
@Time 15.0 sec
>= 90
@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 34
@Time 15.0 sec
34
@Time 0.00417 hour
ASTM D2240
Film Elongation at Break, MD >= 800 %>= 800 %ASTM D882
Film Tensile Strength at Break, MD 7.58 MPa1100 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 82.8 °C<= 181 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 55.0 °C131 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Escorene™ Ultra UL 7765 Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
ExxonMobil EVA 14018.07 Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Eurofoam Evacell EVA 30 EVA + PE Foam
Eurofoam Evacell EVA 100 EVA + PE Foam
ExxonMobil Escorene™ LD 730.09 Molding Ethylene Vinyl Acetate Copolymer

PEX99066 / 175302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.