MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Monprene® CP-19013 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-19013 is a general purpose thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-19013 is a low hardness, low density grade that is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Good Colorability; Good Flexibility; Good Moldability; Good Toughness; Halogen Free; High Elongation; Low Density; Low Hardness; Resilient; Soft

Uses: Closures; Consumer Applications; Diaphragms; Flexible Grips; Gaskets; General Purpose; Handles; Knobs; Luggage; O-rings; Packaging; Rubber Replacement; Safety Equipment; Seals; Soft Touch Applications; Tubing

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 150 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 302 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1515ASTM D2240
 13
@Time 5.00 sec
13
@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 3.10 MPa450 psiASTM D412
Tensile Stress at Strain 0.440 MPa
@Strain 300 %
63.8 psi
@Strain 300 %
ASTM D412
Elongation at Break 830 %830 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 199 - 249 °C390 - 480 °FMelt, Injection
Rear Barrel Temperature 182 - 232 °C360 - 450 °FInjection
Middle Barrel Temperature 188 - 238 °C370 - 460 °FInjection
Front Barrel Temperature 193 - 243 °C380 - 470 °FInjection
Nozzle Temperature 199 - 249 °C390 - 480 °FInjection
Zone 1 182 - 232 °C360 - 450 °FExtrusion
Zone 2 188 - 238 °C370 - 460 °FExtrusion
Zone 3 193 - 243 °C380 - 470 °FExtrusion
Zone 4 193 - 243 °C379 - 469 °FExtrusion
Zone 5 199 - 249 °C390 - 480 °FExtrusion
Die Temperature 199 - 249 °C390 - 480 °FExtrusion
Mold Temperature 35.0 - 48.9 °C95.0 - 120 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Monprene® CP-10130H Thermoplastic Elastomer
Teknor Apex Monprene® SP-39250G CLR XRD2 Thermoplastic Elastomer
Teknor Apex Monprene® MP-2315 Thermoplastic Elastomer
Teknor Apex Monprene® MP-1442A Thermoplastic Elastomer
Teknor Apex Monprene® CP-37225 Thermoplastic Elastomer

PTEKNQ0803 / 237294

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.