MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sibur Nitrilast-26 Nitrile-Butadiene Rubber (NBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: 2895 BAYER. For production of oil-benzene resistant articles for the automobile, aviation and rubber technical industries. Rubbers on the base of Nitrilast possess good oil-benzene resistance. Rubber mixtures on the base of Nitrilast are more resistant to wearing than those made of natural rubber.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 80 - 120
@Temperature 100 °C
80 - 120
@Temperature 212 °F
ML 1-4
Ash <= 0.60 %<= 0.60 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 24.0 MPa>= 3480 psi
Elongation at Break >= 425 %>= 425 %
 
Descriptive Properties
Loss During Drying0.01
Mass Share Adigol-20.5-1.2%
Mass Share of VS-30A1-1.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATG s.r.l. NBR Nitrile-Butadiene Rubber
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Sibur Nitrilast-26M Nitrile-Butadiene Rubber (NBR)
ATG s.r.l. HNBR Hydrogenated Nitrile Butadiene Rubber
Klinger Thermoseal Klinger® Quantum Hydrogenated Nitrile Butadiene Rubber (HNBR)

PSIB107 / 67670

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.