MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nylene® Nylene 5150 HS Nylon 66, 50% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: 50% glass fiber reinforced, heat-stabilized nylon 6/6 injection molding resin. Formulated to exhibit maximum stiffness for the most demanding applications. Should be used in parts and tools specifically designed to accommodate such high glass fiber loadings, in order to maximize part performance.

Testing conducted on dry as molded specimen at 73°F

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.56 g/cc1.56 g/ccASTM D792
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 193 MPa28000 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Modulus 10.07 GPa1461 ksiASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 254 °C489 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Esstech X-951-0050 BisGMA/Triethyleneglycol Dimethacrylate (50/50)
Nylene® PA6/6 Glass Filled 5150 HS Nylon 6/6
Lord Adhesives Chemlok® 5150 Adhesive
Ipiranga Petrochem GF 5150 HDPE
Ipiranga Petrochem GD 5150 K HDPE

PNYLEN967 / 221499

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.