System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
ALIMEX 2017A T451 Aluminum Alloy Rolled
Categories:
Metal
;
Nonferrous Metal
;
Aluminum Alloy
;
2000 Series Aluminum Alloy
Material Notes:
Rolled aluminium material according to DIN EN standard.
Information provided by ALIMEX GmbH
Solution heat treated, stress relieved by stretching a controlled amount and then naturally aged.
Key Words:
EN AW-2017A (AlCu4MgSi)
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
2.801
g/cc
0.1012
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Brinell
>= 105
>= 105
Tensile Strength, Ultimate
370
-
390
MPa
53700
-
56600
psi
Rm
Tensile Strength, Yield
>=
240
MPa
@Strain 0.2 %
>=
34800
psi
@Strain 0.2 %
Elongation at Break
<= 15 %
<= 15 %
Modulus of Elasticity
70.0
GPa
10200
ksi
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.00000357
-
0.00000556
ohm-cm
0.00000357
-
0.00000556
ohm-cm
Thermal Properties
Metric
English
Comments
CTE, linear
23.0
µm/m-°C
@Temperature 20.0 °C
12.8
µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity
130.0
-
200.0
W/m-K
902.2
-
1388
BTU-in/hr-ft²-°F
Descriptive Properties
Corrosion Resistance
Sufficient
Machinability
Good
Protective Anodizing
Good, not decorative
Welding Properties (WIG, MIG)
Less Suitable
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Aluminum 2017A Composition Spec
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Aluminum 2017-T4; 2017-T451
AISI 303 Cast Stainless Steel, EN 10088
ALIMEX PLANAL 5083 O/H111 Aluminum Alloy
NALIMEX10 / 14765
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.