MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.

Data provided by the manufacturer, Special Metals.

Key Words: C-276
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1056 MPa153200 psi
Tensile Strength, Yield 903.9 MPa
@Strain 0.2 %
131100 psi
@Strain 0.2 %
Elongation at Break 32 %32 %
Modulus of Elasticity 205 GPa29700 ksi
Poissons Ratio 0.3070.307
Shear Modulus 79.0 GPa11500 ksi
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability 1.00021.0002at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.427 J/g-°C0.102 BTU/lb-°F
Thermal Conductivity 9.80 W/m-K68.0 BTU-in/hr-ft²-°F
Melting Point 1325 - 1370 °C2417 - 2500 °F
Solidus 1325 °C2417 °F
Liquidus 1370 °C2500 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.010 %<= 0.010 %
Chromium, Cr 14.5 - 16.5 %14.5 - 16.5 %
Cobalt, Co <= 2.5 %<= 2.5 %
Iron, Fe 4.0 - 7.0 %4.0 - 7.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 15 - 17 %15 - 17 %
Nickel, Ni 59 %59 %As remainder
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 0.080 %<= 0.080 %
Sulfur, S <= 0.030 %<= 0.030 %
Vanadium, V <= 0.35 %<= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 718
Special Metals INCONEL® C276 Nickel Superalloy Plate
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work
Special Metals INCONEL® C276 Nickel Superalloy Tubing, Annealed

NINCO03 / 17436

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.