MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources TP-M30 Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Mineral Filled

Material Notes: Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm0.0060 - 0.010 in/inASTM D955
Melt Flow 10 - 15 g/10 min
@Load 2.16 kg,
Temperature 250 °C
10 - 15 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.3 MPa7000 psiASTM D638
Tensile Strength, Yield 51.0 MPa7400 psiASTM D638
Flexural Strength 93.1 MPa13500 psiASTM D790
Flexural Modulus 3.28 GPa475 ksiASTM D790
Izod Impact, Notched 0.747 J/cm
@Temperature 22.8 °C
1.40 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C180 °FASTM D648
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0626 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 243 - 254 °C470 - 490 °F
Middle Barrel Temperature 249 - 260 °C480 - 500 °F
Front Barrel Temperature 254 - 266 °C490 - 510 °F
Melt Temperature 254 - 277 °C490 - 530 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 116 - 121 °C240 - 250 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00254 cm0.00100 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® TPX-PBT-98010 BN069
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage
Overview of materials for Thermoset Polyester Glass Filled BMC
Overview of materials for Thermoset Polyester Glass and Mineral Filled BMC

PPOLYQ273 / 160798

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.