MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Zytel® RS 3061HSL BK039A PA610  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Unreinforced, Renewably Sourced, Polyamide 610 Developed for Injection Molding

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³DAM; ISO 1183
Water Absorption 3.8 %
@Thickness 2.00 mm
3.8 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.70 %
@Thickness 2.00 mm
1.70 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psi50% RH; ISO 527-1/-2
 68.0 MPa9860 psiDAM; ISO 527-1/-2
Elongation at Yield 4.5 %4.5 %DAM; ISO 527-1/-2
 25 %25 %50% RH; ISO 527-1/-2
Tensile Modulus 1.38 GPa200 ksi50% RH; ISO 527-1/-2
 2.40 GPa348 ksiDAM; ISO 527-1/-2
Poissons Ratio 0.380.38DAM; ISO 527-1/-2
 0.430.4350%RH; ISO 527-1/-2
Izod Impact, Unnotched (ISO)  4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 6.30 kJ/m²
@Temperature 23.0 °C
3.00 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched 3.40 J/cm²
@Temperature 23.0 °C
16.2 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.470 J/cm²
@Temperature 23.0 °C
2.24 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.850 J/cm²
@Temperature 23.0 °C
4.04 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+13 ohm-cm2.00e+13 ohm-cm50% RH; IEC 62631-3-1
 >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm50% RH; IEC 62631-3-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 50.0 °C122 °F10°C/min; 50% RH; ISO 11357-1/-2
 60.0 °C140 °F10°C/min; DAM; ISO 11357-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °FInjection
 270 °C518 °FInjection Optimum
Mold Temperature 60.0 - 100 °C140 - 212 °FInjection
 80.0 °C176 °FInjection Optimum
Drying Temperature 80.0 °C176 °FInjection
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.10 %0.10 %Injection
 
Descriptive Properties
AdditivesLubricants
 Release agent
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking Code>PA610<ISO 11469
ProcessingInjection Molding
Resin IdentificationPA610ISO 1043
Special characteristicsHeat stabilized or stable to heat
 Light stabilized or stable to light

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Crastin® S600F20 NC010 PBT
Celanese Zytel® BM7300THS BK317 PA6-HI
Celanese Zytel® RS LC3060 NC010 PA6.10
Celanese Zytel® ST7301 BK356 PA6-HI
DuPont Mobility and Materials Crastin® 6129 NC010 PBT

PZDSX5490 / 198130

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.