MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Lupolen 1800 H LDPE, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Injection moldings

Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³
Water Absorption 0.010 %0.010 %
Moisture Absorption at Equilibrium 0.010 %0.010 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 9.00 MPa1310 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 15.5 %15.5 %
Tensile Modulus 0.200 GPa29.0 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  2.3
@Frequency 100 Hz
2.3
@Frequency 100 Hz
 2.3
@Frequency 1e+6 Hz
2.3
@Frequency 1e+6 Hz
Dissipation Factor 0.00020
@Frequency 100 Hz
0.00020
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 230 µm/m-°C
@Temperature 20.0 °C
128 µin/in-°F
@Temperature 68.0 °F
Melting Point 108 °C226 °F
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C106 °F
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Oxygen Index 17 %17 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 1800 S LDPE, Injection Molding Grade
Overview of materials for Low Density Polyethylene (LDPE), Molded
Braskem PB 608 LDPE Injection Molding Polyethylene
Braskem PB 208 LDPE Injection Molding Polyethylene
Braskem IP2418 LDPE Injection Molding Polyethylene

PSF024 / 66601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.