MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

KaMin Hydramatte® Kaolin Clay - Filler
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Hydramatte® is a coarse delaminated clay designed for low gloss applications such as matte and dull finishes.

Industry: PAPER & PACKAGING

Uses: Coated Freesheet/Art Paper, Coated 1S Label, Coated Bleached Board, Coated Recycle Board, Coated Natural Kraft, Lightweight Coated Paper, Coated Groundwood, Thermal Paper, Uncoated Freesheet, Uncoated Groundwood

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 66 - 68 %66 - 68 %Slurry
Brightness 87.5 - 89 %87.5 - 89 %Reflectance (TAPPI)
Moisture Absorption at Equilibrium <= 1.5 %<= 1.5 %As Produced
Particle Mesh Size 325 Mesh325 Mesh0.005% Retained
pH 6 - 86 - 8100 g/250 ml H2O Slurry
Brookfield Viscosity 800 cP
@Temperature 25.0 °C
800 cP
@Temperature 77.0 °F
20 RPM
 
Descriptive Properties
CAS Number1332-58-7
Physical FormsDry, Slurry
Shipping PointMacon, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KaMin Hydraprint® Kaolin Clay - Filler
KaMin Hydragloss® Clay
KaMin KaMin® HG Kaolin Clay - Waterwashed
KaMin Polyfil® DL Kaolin Clay - Delaminated
KaMin Polyplate® HMT Kaolin Clay - Delaminated

CKAMAN907 / 178378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.