MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® KL 1-2403/40 H1.0 000000 Nylon 6 (PA6), 40% Mineral Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Mineral Filled

Material Notes: 40% mineral

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.446 g/cc0.05224 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.7 %1.7 %50% RH; IOS 62
Water Absorption at Saturation 4.5 %4.5 %IOS 62
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/in150x105x3; ISO 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/in150x105x3; ISO 2577
Melt Flow 31 g/10 min
@Load 5.00 kg,
Temperature 280 °C
31 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 140 MPa20300 psiISO 2093-1
Tensile Strength at Break 65.0 MPa9430 psi5 mm/min; ISO 527-1,-2
Elongation at Break 28 %28 %5 mm/min; ISO 527-1,-2
Tensile Modulus 2.70 GPa392 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 85.0 MPa12300 psi2 mm/min; ISO 178-A
Flexural Yield Strength 65.0 MPa
@Strain 3.5 %
9430 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 2.60 GPa377 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 9.0 %9.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  70.0 kJ/m²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 <= 1.00 J/cm²
@Temperature -40.0 °C
<= 4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 180-1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 ohm-cm1.00e+9 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant  5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 60250
 10
@Frequency 100 Hz
10
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor 0.15
@Frequency 100 Hz
0.15
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °F10°C/min; ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 °C572 °F
Mold Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® DP 1801/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Mitsubishi Lemalloy® C61HL PPE-PA66 Alloy
Mitsubishi Lemalloy® BX528A-3 PPE-PA6 Alloy
Mitsubishi Lemalloy® BX503A-1 PPE-PA6 Alloy
Envalior Durethan® BC 40 SR2 000000 Nylon 6 (PA6), Dry

PLANW9571 / 208371

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.