MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Pignut Hickory Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Carya glabra; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.660 g/cc0.0238 lb/in³Oven Dry Weight/Unseasoned Volume
 1.03 g/cc0.0370 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0807 GPa11.7 ksiStatic Bending*
Flexural Yield Strength 42.7 MPa6200 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 11.4 GPa1650 ksiStatic Bending*
Compressive Strength 7.86 MPa1140 psiPerpendicular to Grain*
 27.2 MPa3950 psiParallel to Grain*
 33.2 MPa4810 psiMax Crushing Strength Parallel to Grain*
Shear Strength 9.45 MPa1370 psiParallel to Grain*
Impact 8.88.8in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 1690016900psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00924 J/cm³1.34 in-lb/in³Static Bending*
Work to Maximum Load 0.219 J/cm³31.7 in-lb/in³Static Bending*
 
Thermal PropertiesMetricEnglishComments
Shrinkage 7.2 %7.2 %Tangential; Unseasoned to Oven Dry*
 7.2 %7.2 %Radial, from green to oven dry
 11.5 %11.5 %Tangential, from green to oven dry
 17.9 %17.9 %Volumetric, from green to oven dry
 18.2 %18.2 %Radial; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexTow® AS4C 12K Standard Modulus Carbon Fiber (12,000 Filaments)
American Pecan Hickory Wood
Hexcel® HexTow® AS4C 6K Standard Modulus Carbon Fiber (6000 Filaments)
Silver Maple (Water Maple, White Maple), Soft Wood
European Field Elm Wood

PTSA050 / 71243

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.