MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Moplen HP553P Fiber (Staple) Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Moplen HP553P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP553P is a homopolymer typically used by customers in high speed production of staple fiber. Moplen HP553P resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Features: Excellent spinnability; Excellent drawability; Anti-gas fading; Outstanding gloss and surface appearance

Applications: Staple Fiber for diaper and sanitary napkin; Geotextile; Industrial

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
14 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104104ASTM D785
Tensile Strength, Yield 37.3 MPa5400 psiASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Modulus 1.47 GPa213 ksiASTM D790
Izod Impact, Notched 0.392 J/cm0.735 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accucomp Polypropylene HPO306L Homopolymer
Envalior EcoPaXX® Q-KV PA410 FR, Dry, Flame Retardant
Aclo Accutech Polypropylene CP0437T40V Copolymer Talc Reinforced
Aclo Accutech Polypropylene CP0435G20HIV Copolymer Glass Reinforced High Impact
Aclo Accutech Polypropylene CP0409HUUVV Copolymer UV Stabilized

PMIRAE42 / 53154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.