MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

o-Xylene, C8H10
Categories: Fluid; Solvent

Key Words: C8H10
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.876 g/cc
@Temperature 20.0 °C
0.0316 lb/in³
@Temperature 68.0 °F
Viscosity 0.802 cP
@Temperature 20.0 °C
0.802 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 106.168 g/mol106.168 g/mol
Vapor Pressure 0.006507 bar
@Temperature 20.0 °C
4.881 torr
@Temperature 68.0 °F
Surface Tension 29.49 dynes/cm
@Temperature 20.0 °C
29.49 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 37.3 bar28000 torr
Critical Temperature 357 °C675 °F
Critical Density 0.288 g/cc0.0104 lb/in³
Critical Molar Volume 369 cm³/mol22.5 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.568
@Temperature 20.0 °C
2.568
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 346.8 J/g149.2 BTU/lb
Specific Heat Capacity 1.771 J/g-°C0.4233 BTU/lb-°F
 1.255 J/g-°C
@Temperature 25.0 °C
0.3000 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Melting Point -25.2 °C-13.4 °F
Boiling Point 144.5 °C292.1 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.503
@Wavelength 589.3 nm
1.503
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.1156
Antoine's Vapor Pressure B Parameter3395.57
Antoine's Vapor Pressure C Parameter-59.46
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)95-47-6
Chemical FormulaC8H10
Critical Compressibility (Zc)0.263
Dipole moment (p/C.m)1.668E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A513.54
Dynamic Viscosity Parameter B277.98
Henry's Law Constant (atm m3/mol)0.00519
Molar Heat Capacity (298K)133.204 J/mol-K
Molar Heat Capacity of Vapor a Parameter-15.8406
Molar Heat Capacity of Vapor b Parameter0.5958
Molar Heat Capacity of Vapor c Parameter-0.0003441
Molar Heat Capacity of Vapor d Parameter7.523E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1307
UV cut-off (nm)290

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
1-Pentanol, C5H12O
1-Octanol, C8H18O

VORGS381 / 99726

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.