MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³
Linear Mold Shrinkage, Flow 0.0035 - 0.0060 cm/cm0.0035 - 0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0075 - 0.0105 cm/cm0.0075 - 0.0105 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  90.0 MPa
@Temperature 150 °C
13100 psi
@Temperature 302 °F
 105 MPa
@Temperature 120 °C
15200 psi
@Temperature 248 °F
 115 MPa
@Temperature 90.0 °C
16700 psi
@Temperature 194 °F
 145 MPa
@Temperature 60.0 °C
21000 psi
@Temperature 140 °F
 185 MPa
@Temperature 23.0 °C
26800 psi
@Temperature 73.4 °F
Elongation at Break  2.8 %
@Temperature 23.0 °C
2.8 %
@Temperature 73.4 °F
 3.5 %
@Temperature 60.0 °C
3.5 %
@Temperature 140 °F
 4.7 %
@Temperature 90.0 °C
4.7 %
@Temperature 194 °F
 5.2 %
@Temperature 120 °C
5.2 %
@Temperature 248 °F
 5.6 %
@Temperature 150 °C
5.6 %
@Temperature 302 °F
Tensile Modulus  4.90 GPa
@Temperature 150 °C
711 ksi
@Temperature 302 °F
 6.20 GPa
@Temperature 120 °C
899 ksi
@Temperature 248 °F
 8.30 GPa
@Temperature 90.0 °C
1200 ksi
@Temperature 194 °F
 9.50 GPa
@Temperature 60.0 °C
1380 ksi
@Temperature 140 °F
 10.5 GPa
@Temperature 23.0 °C
1520 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °F
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °F
Vicat Softening Point 255 °C
@Load 5.00 kg
491 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 - 300 °C527 - 572 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
194 - 212 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Dry)
DuPont Mobility and Materials Zytel® 70G35HSL BK039B PA66-GF35
LATI Latamid 66 PA 66
Domo TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY
Celanese Zytel® 70G35EF BK538 PA66-GF35

PLATH9715 / 177411

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.