MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makroblend® DP 2-7655 Polycarbonate + PET, Mineral Filled Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:
  • Developmental product
  • ISO 7792-1-PC/PET,MHPR,-030,MD10
  • (PC+PET)-blends
  • impact modified
  • Injection molding grade 10% mineral filled

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Melt Density 1.11 g/cc
@Temperature 270 °C
0.0401 lb/in³
@Temperature 518 °F
Water Absorption 0.90 %0.90 %Similar to ISO 62
Moisture Absorption at Equilibrium 0.20 %0.20 %Similar to ISO 62
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 260 °C
11 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 3.00 GPa435 ksiISO 527-1/-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
 3.5
@Frequency 100 Hz
3.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 36.0 kV/mm914 kV/inIEC 60243-1
Dissipation Factor  0.0038
@Frequency 100 Hz
0.0038
@Frequency 100 Hz
IEC 60250
 0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 1.71 J/g-°C0.409 BTU/lb-°FMelt
Thermal Conductivity 0.196 W/m-K1.36 BTU-in/hr-ft²-°FMelt
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 111 °C232 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 23 %23 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F
 270 °C518 °FInjection Molding; ISO 294
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
 70.0 °C158 °FInjection Molding; ISO 10724
Ejection Temperature 170 °C338 °F
Injection Velocity 200 mm/sec7.87 in/secISO 294
Drying Temperature 110 °C230 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourDry air dryer
 2.00 - 3.00 hour2.00 - 3.00 hourFresh air dryer (high speed dryer)
 4.00 - 8.00 hour4.00 - 8.00 hourCirculating air drying oven (50 % fresh air)
Moisture Content <= 0.010 %<= 0.010 %
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America
Eff. thermal diffusivity (m²/s)1.04E-07
FeatureRelease agent
FormPellets
ProcessInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® DP 2-7655 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade
Covestro Makroblend® UT305 PC/PET Blend
Aclo Acculoy POL062L Polycarbonate PET Alloy
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized

PB09832 / 92672

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.