MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Envalior Stanyl® TW271F6 (PA46+PTFE)-GF30, Dry, 30% Glass Fiber, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46)

Material Notes: 30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ISO 1183
Moisture Absorption 2.00 %2.00 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 190 MPa27600 psiISO 527-1/-2
 75.0 MPa
@Temperature 200 °C
10900 psi
@Temperature 392 °F
ISO 527-1/-2
 80.0 MPa
@Temperature 180 °C
11600 psi
@Temperature 356 °F
ISO 527-1/-2
 85.0 MPa
@Temperature 160 °C
12300 psi
@Temperature 320 °F
ISO 527-1/-2
 100 MPa
@Temperature 120 °C
14500 psi
@Temperature 248 °F
ISO 527-1/-2
Elongation at Break 3.5 %3.5 %ISO 527-1/-2
 6.5 %
@Temperature 120 °C
6.5 %
@Temperature 248 °F
ISO 527-1/-2
 6.5 %
@Temperature 160 °C
6.5 %
@Temperature 320 °F
ISO 527-1/-2
 6.5 %
@Temperature 180 °C
6.5 %
@Temperature 356 °F
ISO 527-1/-2
 6.5 %
@Temperature 200 °C
6.5 %
@Temperature 392 °F
ISO 527-1/-2
Tensile Modulus 10.0 GPa1450 ksiISO 527-1/-2
 4.25 GPa
@Temperature 200 °C
616 ksi
@Temperature 392 °F
ISO 527-1/-2
 4.50 GPa
@Temperature 180 °C
653 ksi
@Temperature 356 °F
ISO 527-1/-2
 4.75 GPa
@Temperature 160 °C
689 ksi
@Temperature 320 °F
ISO 527-1/-2
 5.25 GPa
@Temperature 120 °C
761 ksi
@Temperature 248 °F
ISO 527-1/-2
Flexural Modulus 8.50 GPa1230 ksiISO 178
Izod Impact, Notched (ISO)  11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  6.50 J/cm²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Comparative Tracking Index 400 V400 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-1/-2
Melting Point 295 °C563 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FISO 72-1/-2
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TW271F6 (PA46+PTFE)-GF30, Conditioned, 30% Glass Fiber, Heat Stabilized
Delrin Delrin® 100P NC010 POM
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxide Filled
Envalior Stanyl® TW271F6J10 (PA46+PTFE)-GF30
Bethlehem Steel ASTM A36, 3/16 to 3/4 in. thick, as-rolled steel plate

PDSM8252 / 184953

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.