MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 7055-T7751 Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: This alloy was specifically developed for use in compression-dominated structures and provides advantages over alloy 7150 in compressive and tensile strengths while maintaining other important properties such as fracture toughness and corrosion resistance.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Information provided by Alcoa and the reference(s).

Key Words: UNS A97055; Aluminium 7055-T7751; AA7055; Al7055-T7751
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.86 g/cc0.103 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  634 MPa
@Thickness 25.4 mm
92000 psi
@Thickness 1.00 in
Longitudinal Direction
 641 MPa
@Thickness 25.4 mm
93000 psi
@Thickness 1.00 in
LT Direction
Tensile Strength, Yield  614 MPa
@Thickness 25.4 mm
89000 psi
@Thickness 1.00 in
Longitudinal Direction
 614 MPa
@Thickness 25.4 mm
89000 psi
@Thickness 1.00 in
LT Direction
Elongation at Break  10 %
@Thickness 25.4 mm
10 %
@Thickness 1.00 in
LT Direction
 11 %
@Thickness 25.4 mm
11 %
@Thickness 1.00 in
Longitudinal Direction
Compressive Yield Strength  621 MPa
@Thickness 25.4 mm
90000 psi
@Thickness 1.00 in
Longitudinal Direction
 648 MPa
@Thickness 25.4 mm
94000 psi
@Thickness 1.00 in
LT Direction
Fracture Toughness  26.4 MPa-m½
@Thickness 25.4 mm
24.0 ksi-in½
@Thickness 1.00 in
KIC, T-L
 28.6 MPa-m½
@Thickness 25.4 mm
26.0 ksi-in½
@Thickness 1.00 in
KIC, L-T
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 85.9 - 88.5 %85.9 - 88.5 %As remainder
Chromium, Cr <= 0.04 %<= 0.04 %
Copper, Cu 2.0 - 2.6 %2.0 - 2.6 %
Iron, Fe <= 0.15 %<= 0.15 %
Magnesium, Mg 1.8 - 2.3 %1.8 - 2.3 %
Manganese, Mn <= 0.05 %<= 0.05 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.10 %<= 0.10 %
Titanium, Ti <= 0.06 %<= 0.06 %
Zinc, Zn 7.6 - 8.4 %7.6 - 8.4 %
Zirconium, Zr 0.08 - 0.25 %0.08 - 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7055-T77511 Extrusions
Aluminum 7075-T6; 7075-T651
Aluminum 7150-T7751 Plate
Alcoa 7055-T77511 Aluminum Extrusions
Alcoa 7055-T7751 Aluminum Plate

MA7055 / 9581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.