MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40, 20/20% Glass/Glass Beads Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Glass Bead Filled

Material Notes: 20% Glass Reinforced, 20% Beads Reinforced

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³ISO 1183
Water Absorption 0.15 %0.15 %Sim. ISO 62
Moisture Absorption 0.250 %0.250 %Humidity; Sim. ISO 62
Viscosity  18 cP
@Shear Rate 100000 1/s,
Temperature 250 °C
18 cP
@Shear Rate 100000 1/s,
Temperature 482 °F
 19 cP
@Shear Rate 100000 1/s,
Temperature 270 °C
19 cP
@Shear Rate 100000 1/s,
Temperature 518 °F
 20 cP
@Shear Rate 100000 1/s,
Temperature 230 °C
20 cP
@Shear Rate 100000 1/s,
Temperature 446 °F
 200 cP
@Shear Rate 1000 1/s,
Temperature 270 °C
200 cP
@Shear Rate 1000 1/s,
Temperature 518 °F
 230 cP
@Shear Rate 1000 1/s,
Temperature 250 °C
230 cP
@Shear Rate 1000 1/s,
Temperature 482 °F
 240 cP
@Shear Rate 10 1/s,
Temperature 270 °C
240 cP
@Shear Rate 10 1/s,
Temperature 518 °F
 300 cP
@Shear Rate 10 1/s,
Temperature 250 °C
300 cP
@Shear Rate 10 1/s,
Temperature 482 °F
 300 cP
@Shear Rate 1000 1/s,
Temperature 230 °C
300 cP
@Shear Rate 1000 1/s,
Temperature 446 °F
 500 cP
@Shear Rate 10 1/s,
Temperature 230 °C
500 cP
@Shear Rate 10 1/s,
Temperature 446 °F
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inSim. to ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inSim. to ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiISO 527-1/-2
Elongation at Break 2.5 %2.5 %ISO 527-1/-2
Tensile Modulus 9.10 GPa1320 ksiISO 527-1/-2
Charpy Impact Unnotched  3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 130 µm/m-°C72.2 µin/in-°FISO 11359-1/-2
Melting Point 225 °C437 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 72-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 72-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Arnite® TV4 640 (PBT+PC) - GF20
Envalior Arnite® TZ6 280 PBT-(GF+GB)40, 20/20% Glass/Glass Beads Filled
Chang Chun Plastic PBT1200M General Purpose PBT
Chang Chun Plastic PBT1100L General Purpose PBT
Envalior Arnite® TV4 441 (PBT+PET)-GF20

PDSM8144 / 184845

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.