MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Garlock THERMA-PUR™ 4122-CMG High Temperature Gasketing Material
Categories: Metal

Material Notes: THERMa-PUR™ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a unique formulation with a patent-pending core.
  • Able to withstand high temperature, whether continuous or in thermal cycling conditions
  • Excellent oxidation resistance
  • Hydrophobic and electrically insulating
  • Easy release from flanges
4122-CMG: Corrugated Metal Gasket

Information provided by Garlock Rubber Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0492 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 8.27 MPa1200 psiASTM F152
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 3.94 kV/mm100 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1000 °C
@Pressure 6.89 MPa
1832 °F
@Pressure 1000 psi
Continuous
 
Descriptive Properties
Compressibility, %34-45ASTM F36
Creep Relaxation, %25ASTM F38

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Garlock GRAPH-LOCK® 3128 HOCHDRUCK® Graphite Sheet Gasketing, Steel Reinforced
Garlock GYLON® 3530 PTFE Gasketing, Graphite Filler
Garlock THERMA-PUR™ 4122-KAMM High Temperature Gasketing Material
Garlock GRAPH-LOCK® 3124/3126 Graphite Sheet Gasketing, Steel Wire Insert
Garlock GRAPH-LOCK® 3123/3125 Graphite Sheet Gasketing

PGARL835 / 157515

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.