MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

Klinger Thermoseal ML-5270 PTG Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Chlorosulfonated Polyethylene Rubber

Material Notes: Thermoseal ML-5270 is a high performance synthetic fiber and polychloroprene binder gasket material that is resistant to refrigerants and oil mixtures. Its unique Multi-Layer Technology structure provides exceptional low flange pressure sealability with exceptional torque retention. Multi-Layer Technology sheet products consist of a reinforced high density core with conformable sealing layers on each side. Typical applications include gaskets in hermetic and semi-hermetic compressors and oil pan gaskets in heavy-duty diesel engines with intermittent operating temperatures up to 350° F (177° C).

Data for this material is available for download into ANSYS xml format: C5270; 1/32" (right click and "save as" to download)

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ASTM F1315
Thickness 1588 microns62.52 milThickness tested
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 15.5 MPa2250 psiASTM F152
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °Fintermittent
 
Descriptive Properties
Compressibility8-14 percentASTM F36J
Creep<30%1/32", ASTM F38B
Pressure<800 psi
Recovery>40 percentASTM F36J
Sealability<0.20 ml/hrASTM F37
Thickness Increase<30%After immersion in Oil IRM903 for 5 hrs. at 300° F (149°), ASTM F146
 0-5%After immersion in ASTM Oil #1 for 5 hrs. at 300° F (149° C), After immersion in ASTM Oil #1 for 5 hrs. at 300° F (149° C)
 5-10%After immersion in Fuel A for 5 hrs. at 73° F (23° C), ASTM F146
Weight Increase<15%ASTM F146, After immersion in Fuel B for 5 hrs. at 73° (23° C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Klinger Thermoseal KLINGERSIL® C-4401 General Application Gasketing
Klinger Thermoseal ML-N562 PTG Gasketing
Ductile Iron tension grade 65-45-12
Special Metals INCONEL® Alloy 625
AISI 4140 Steel, oil quenched, 100 mm (4 in.) round (845°C (1550°F) quench, 650°C (1200°F) temper)

PTHERM923 / 146077

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.