MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Imerys G-200 HP Feldspar
Categories: Ceramic; Clay; Feldspar Clay; Oxide; Silicon Oxide

Material Notes: G-200 HP Feldspar is a high potassium aluminum silicate ground to 200 mesh for ceramic applications. G-200 HP offers high potassium content and low iron oxide per unit of alumina.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.993 g/cc0.0359 lb/in³loose
 1.19 g/cc0.0428 lb/in³packed
Particle Size 13.3 µm13.3 µm
Particle Mesh Size 200 Mesh200 Mesh0.5% retained
 300 Mesh300 Mesh5% retained
Specific Surface Area 1.2 m²/g1.2 m²/g
 
Component Elements PropertiesMetricEnglishComments
Al2O3 18.2 %18.2 %
CaO 0.75 %0.75 %
Fe2O3 0.090 %0.090 %
K2O 13.2 %13.2 %
Loss on Ignition(%) 0.16 %0.16 %
Na2O 1.52 %1.52 %
SiO2 65.9 %65.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Imerys G-20 HP Feldspar
Imerys Minsilspar™ Feldspar
Imerys G-40 HP Feldspar
Omya OMYAFLOW® 3 - SY Calcium Carbonate
Imerys Minspar™ 250 Feldspar

CIMERY003 / 88353

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.