MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poco Graphite EDM-3 EDM Graphite
Categories: Carbon; Graphite

Material Notes: POCO's EDM-3 is an isotropic Ultrafine grain graphite which offers high strength with outstanding wear and fine surface finish characteristics easily machined to thicknesses of .005 or less.

Applications:
EDMing of fine detailed electrodes
Punch & die sets
Plastic injection molds
Threading electrodes
Use in aerospace metal cutting

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size <= 5.0 µm<= 5.0 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373
Flexural Strength 91.7 MPa13300 psi
Compressive Strength 125 MPa18100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00156 ohm-cm0.00156 ohm-cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Poco Graphite EDM-AF5 EDM Graphite
Poco Graphite EDM-1 EDM Graphite
Poco Graphite EDM-C3 EDM Graphite
Graphite, Carbon, C
NeoGraf eGRAF® HITHERM™ HT-1220 Graphite

CPOCO02 / 85579

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.