MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Vycom VINTEC I® PVC Polyvinyl Chloride (PVC)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical resistance is necessary. Its high strength-to-weight ratio, cost efficiency, ease of fabrication and economic balance make it the material of choice. Vintec I conforms to ASTM D-1784-95 Class 12454-B (Formerly Type I Grade 1) and is manufactured without the use of plasticizers or fillers. It can be used in self supporting construction up to 140º F (depending on chemistry). It exhibits excellent fire ratings (UL-94V-0) and has a flame spread under 20 per ASTM-E-84. Vintec I is available in numerous colors, finishes and sizes.

FEATURES AND BENEFITS

  • Strength- Vintec I combines tensile strength and stiffness for the toughest applications.
  • Chemical Resistance- Vintec I is resistant to most acids and alkali solutions.
  • Workability- Vintec I can be machined, cut, welded and glued for fabrication versatility.
  • Low Cost- Vintec I is an economical choice for fabricating equipment, tanks, pumps etc.
  • Consistency- Vintec I is extruded through most of the available gauges for dimensional consistency.
  • Flammability- Vintec I is self extinguishing.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ASTM D792
Water Absorption 0.060 %0.060 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Hardness, Shore D 8989ASTM D2240
Tensile Strength, Yield 51.7 MPa7500 psiASTM D638
Tensile Modulus 2.83 GPa411 ksiASTM D638
Flexural Yield Strength 88.3 MPa12800 psiASTM D790
Flexural Modulus 3.32 GPa481 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.40e+15 ohm-cm5.40e+15 ohm-cmASTM D257
Dielectric Constant 3.19
@Frequency 60 Hz
3.19
@Frequency 60 Hz
ASTM D150
Dielectric Strength 21.4 kV/mm544 kV/inASTM D149
Dissipation Factor 0.0096
@Frequency 60 Hz
0.0096
@Frequency 60 Hz
ASTM D150
Dielectric Loss Index 0.0300.030ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 57.6 µm/m-°C
@Temperature 20.0 °C
32.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C179 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FASTM D648
Vicat Softening Point 82.8 °C181 °FASTM D1525
Flammability, UL94 V-0V-0
Flame Spread Index 1515ASTM E84
 
Descriptive Properties
Chemical ResistanceClass BASTM D1784
FlammabilitySelf-ExtinguishingASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC)
Overview of materials for PVC, Molded
Overview of materials for Acrylic, Cast
Overview of materials for Acrylic, Extruded
Geon® Performance Solutions 81510 Polyvinyl Chloride, Rigid

PCPCV21 / 29093

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.