MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Sandvik 75X1 Spring Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Sandvik Sanicro 75X1 is an austenitic precipitation hardenable nickel-base alloy with good spring properties up to 600°C and good resistance to gas corrosion at high temperature. It maximum service temperature is dependent on as-delivered condition and heat treatment.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.30 g/cc0.300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 800 MPa116000 psiannealed
 1000 MPa145000 psisoft drawn, 15% final reduction
 1200 MPa174000 psiannealed, post heat treatment
 1600 MPa232000 psihard drawn, 65% final reduction
 1850 MPa268000 psihard drawn, 65% final reduction, post heat treatment
Tensile Strength, Yield  400 MPa
@Strain 0.2 %
58000 psi
@Strain 0.2 %
annealed
 800 MPa
@Strain 0.2 %
116000 psi
@Strain 0.2 %
soft drawn,15% final reduction
 800 MPa
@Strain 2 %
116000 psi
@Strain 2 %
annealed, post heat treatment
 1500 MPa
@Strain 0.2 %
218000 psi
@Strain 0.2 %
hard drawn, 65% final reduction
 1750 MPa
@Strain 2 %
254000 psi
@Strain 2 %
hard drawn, 65% final reduction, post heat treatment
Modulus of Elasticity 180 GPa26100 ksihard drawn, 65% reduction
 193 GPa28000 ksiannealed
 211 GPa30600 ksihard drawn, 65% reduction, post heat treatment
 216 GPa31300 ksiannealed, post heat treatment
Poissons Ratio 0.300.30Calculated
Shear Modulus 70.0 GPa10200 ksihard drawn, 65% reduction
 74.0 GPa10700 ksiannealed
 81.5 GPa11800 ksihard drawn, 65% reduction, post heat treatment
 83.0 GPa12000 ksiannealed, post heat treatment
Shear Strength  170 MPa
@Temperature 1000 - 1050 °C
24700 psi
@Temperature 1830 - 1920 °F
A,B classification
 205 MPa
@Temperature 1150 - 1200 °C
29700 psi
@Temperature 2100 - 2190 °F
C classification
 380 MPa
@Temperature <=500 °C
55100 psi
@Temperature <=932 °F
C classification
 480 MPa
@Temperature <=500 °C
69600 psi
@Temperature <=932 °F
A,B classification
 585 MPa
@Temperature 600 - 700 °C
84800 psi
@Temperature 1110 - 1290 °F
D classification
 690 MPa
@Temperature <=500 °C
100000 psi
@Temperature <=932 °F
D classification
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.000120 ohm-cm
@Temperature 20.0 °C
0.000120 ohm-cm
@Temperature 68.0 °F
 0.000125 ohm-cm
@Temperature 300 °C
0.000125 ohm-cm
@Temperature 572 °F
 0.000130 ohm-cm
@Temperature 700 °C
0.000130 ohm-cm
@Temperature 1290 °F
Magnetic Permeability 1.0041.004µ
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.2 µm/m-°C
@Temperature 20.0 - 100 °C
6.78 µin/in-°F
@Temperature 68.0 - 212 °F
 13.4 µm/m-°C
@Temperature 30.0 - 300 °C
7.44 µin/in-°F
@Temperature 86.0 - 572 °F
 13.8 µm/m-°C
@Temperature 30.0 - 500 °C
7.67 µin/in-°F
@Temperature 86.0 - 932 °F
 16.5 µm/m-°C
@Temperature 30.0 - 900 °C
9.17 µin/in-°F
@Temperature 86.0 - 1650 °F
Specific Heat Capacity  0.420 - 0.460 J/g-°C
@Temperature 20.0 - 100 °C
0.100 - 0.110 BTU/lb-°F
@Temperature 68.0 - 212 °F
 0.540 J/g-°C
@Temperature 50.0 - 900 °C
0.129 BTU/lb-°F
@Temperature 122 - 1650 °F
Thermal Conductivity  16.3 W/m-K
@Temperature 100 °C
113 BTU-in/hr-ft²-°F
@Temperature 212 °F
 37.2 W/m-K
@Temperature 900 °C
258 BTU-in/hr-ft²-°F
@Temperature 1650 °F
Maximum Service Temperature, Air 600 °C1110 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 16 %16 %
Manganese, Mn 0.50 %0.50 %
Nickel, Ni 72 %72 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si 0.30 %0.30 %
Sulfur, S <= 0.015 %<= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik 11R51 Spring Wire
Sandvik 12R10 Spring Wire
Sandvik 5R60/5R62 Spring Wire
Sandvik SAF 2205SH Spring Wire
347 Stainless Steel, cold drawn wire, 75% hard, 3.20-9.53 mm diameter

NSANDV273 / 19167

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.