MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Leaded Yellow Brass, UNS C85400, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications: General purpose yellow casting alloy not subject to high internal pressure. Furniture hardware, ornamental castings, radiator fittings, ship trimmings, cocks, battery clamps, valves and fittings.

Classified under: Yellow brasses and leaded yellow brasses. ASTM B584; formerly ASTM B146-6B

As cast values below are for sand casting. Alloy does not respond to heat treating. Casting shrinkage allowance is 1.5 - 1.8%

Key Words: Leaded yellow brass, No. 1 yellow brass, 67-1-3-29, CA 854, ASTM B30 (CA854), ASTM B271, ASTM B584; ASTM B146-6B, SAE J462, Ingot code no. 400, FED QQ-C-390, MIL-C-15345 (Alloy 23)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.45 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 5050
Tensile Strength, Ultimate 235 MPa34100 psi
Tensile Strength, Yield 83.0 MPa
@Strain 0.5 %
12000 psi
@Strain 0.5 %
Elongation at Break 35 %35 %In 50 mm
Tensile Modulus 82.7 GPa12000 ksi
Machinability 80 %80 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000008796 ohm-cm
@Temperature 20.0 °C
0.000008796 ohm-cm
@Temperature 68.0 °F
19.6% IACS
Magnetic Permeability 1.01.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.2 µm/m-°C
@Temperature 20.0 - 100 °C
11.2 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 88.0 W/m-K
@Temperature 20.0 °C
611 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 925 - 940 °C1700 - 1720 °F
Solidus 925 °C1700 °F
Liquidus 940 °C1720 °F
Shrinkage 1.6 %1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.35 %<= 0.35 %
Copper, Cu 65 - 70 %65 - 70 %
Iron, Fe <= 0.70 %<= 0.70 %
Lead, Pb 1.5 - 3.5 %1.5 - 3.5 %
Nickel, Ni <= 1.0 %<= 1.0 %
Silicon, Si <= 0.050 %<= 0.050 %
Tin, Sn 0.50 - 1.5 %0.50 - 1.5 %
Zinc, Zn 24 - 32 %24 - 32 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Leaded Yellow Brass, UNS C85200, Copper Casting Alloy
Leaded Yellow Brass, UNS C85700, Copper Casting Alloy, Sand and Centrifugal Castings
Aluminum Bronze, UNS C95500, Casting Alloy, As-Cast
Leaded Yellow Brass, UNS C85800, Copper Casting Alloy, Die Castings
Aluminum Bronze, UNS C95300, Casting Alloy, As Cast

MC85400b1 / 11908

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.