MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 31826 Industrial Polyethylene Temporary Surface Protection Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Industrial Polyethylene Temporary Surface Protection Tape 31826 is a very low adhesion temporary protection tape designed for a variety of surface protection applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.2 MPa2490 psiASTM D3759
Elongation at Break 450 %450 %ASTM D3759
Peel Strength 0.07669 kN/m0.4375 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypeAcrylic-Based
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 31825 Industrial Polyethylene Temporary Surface Protection Tape
3M 2A88 Co-Extruded Multi-Polymer Protect Tapes
3M 3188 (Clear) Polyethylene Protective Tapes
3M 3187 (Clear) Polyethylene Protective Tapes
3M 2A87 Co-Extruded Multi-Polymer Protect Tapes

PMM34326 / 169073

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.