MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: Displays Low Temperature Flexibility and Abrasion Resistance.

Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for Lamination

Available in Americas and Asia

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Viscosity 2400 cP2400 cPRVT Spindle #2, 20 rpm, 23°C, 15% TS in Cyclohexanone
 28000 cP
@Temperature 204 °C
28000 cP
@Temperature 399 °F
Melt; ASTM D1084-88
Brookfield Viscosity 475 cP475 cPRVT Spindle #2, 20 rpm, 23°C, 15% TS in THF
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Tensile Strength 49.0 MPa7110 psiASTM D412/D638
Elongation at Break 460 %460 %ASTM D412/D638
100% Modulus 5.20 MPa
@Strain 100 %
754 psi
@Strain 100 %
300% Modulus 13.1 MPa
@Strain 300 %
1900 psi
@Strain 300 %
Peel Strength 0.110 kN/m0.628 pliAdhesion to PET; TP-141
 0.900 kN/m5.14 pliAluminum Foil; ASTM D1867-72
 5.00 kN/m28.5 pliMylar Film; ASTM D1867-72
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 70.0 °C158 °FASTM D1525
Glass Transition Temp, Tg -23.0 °C-9.40 °FDSC
Ring & Ball Softening Point 161 °C322 °FASTM E28-92
 
Descriptive Properties
Gradient Bar Tack Temperature121°C
Open Time<5 secASTM D4497-94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 5708 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane
Lubrizol Estane® 5712 Thermoplastic Polyurethane
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane

PNOVEON010 / 55275

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.