MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin DAI-EL® G-555 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Low-temperature resistance (G558:extrusion)

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.89 g/cc1.89 g/cc
Mooney Viscosity  35
@Temperature 121 °C
35
@Temperature 250 °F
ML1+10
 43
@Temperature 100 °C
43
@Temperature 212 °F
ML1+10
 62
@Temperature 100 °C
62
@Temperature 212 °F
Compound, ML1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7373peak
 63
@Time 3.00 sec
63
@Time 0.000833 hour
 73
@Treatment Temp. 230 °C,
Time 252000 sec
73
@Treatment Temp. 446 °F,
Time 70.0 hour
Air aging test
 74
@Treatment Temp. 250 °C,
Time 252000 sec
74
@Treatment Temp. 482 °F,
Time 70.0 hour
Air aging test
 75
@Treatment Temp. 275 °C,
Time 252000 sec
75
@Treatment Temp. 527 °F,
Time 70.0 hour
Air aging test
Tensile Strength at Break 12.7 MPa1840 psi
 14.1 MPa
@Treatment Temp. 275 °C,
Time 252000 sec
2050 psi
@Treatment Temp. 527 °F,
Time 70.0 hour
Air aging test
 19.5 MPa
@Treatment Temp. 250 °C,
Time 252000 sec
2830 psi
@Treatment Temp. 482 °F,
Time 70.0 hour
Air aging test
 21.9 MPa
@Treatment Temp. 230 °C,
Time 252000 sec
3180 psi
@Treatment Temp. 446 °F,
Time 70.0 hour
Air aging test
Elongation at Break 330 %330 %
 333 %
@Treatment Temp. 230 °C,
Time 252000 sec
333 %
@Treatment Temp. 446 °F,
Time 70.0 hour
Air aging test
 373 %
@Treatment Temp. 250 °C,
Time 252000 sec
373 %
@Treatment Temp. 482 °F,
Time 70.0 hour
Air aging test
 495 %
@Treatment Temp. 275 °C,
Time 252000 sec
495 %
@Treatment Temp. 527 °F,
Time 70.0 hour
Air aging test
100% Modulus 2.70 MPa
@Strain 100 %
392 psi
@Strain 100 %
Tear Strength 30.0 kN/m171 pliangle type
Compression Set  17 %
@Temperature 100 °C,
Time 252000 sec
17 %
@Temperature 212 °F,
Time 70.0 hour
P-24 O-ring
 18 %
@Temperature 150 °C,
Time 252000 sec
18 %
@Temperature 302 °F,
Time 70.0 hour
P-24 O-ring
 21 %
@Temperature 175 °C,
Time 252000 sec
21 %
@Temperature 347 °F,
Time 70.0 hour
P-24 O-ring
 25 %
@Temperature 50.0 °C,
Time 252000 sec
25 %
@Temperature 122 °F,
Time 70.0 hour
P-24 O-ring
 28 %
@Temperature 25.0 °C,
Time 252000 sec
28 %
@Temperature 77.0 °F,
Time 70.0 hour
P-24 O-ring
 29 %
@Temperature 200 °C,
Time 252000 sec
29 %
@Temperature 392 °F,
Time 70.0 hour
P-24 O-ring
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -14.0 °C6.80 °FLow Temperature Retraction, TR10
 -14.0 °C6.80 °FGehman Torsion T10
 -7.00 °C19.4 °FLow Temperature Retraction, TR70
 -4.00 °C24.8 °FGehman Torsion T2
Brittleness Temperature -26.0 °C-14.8 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  5.50 min
@Temperature 160 °C
0.0917 hour
@Temperature 320 °F
MDR, T90
 7.00 min
@Temperature 160 °C
0.117 hour
@Temperature 320 °F
Curelastometer, T90
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 69 %69 %
 
Descriptive Properties
Test Formula100Polymer
 13N774 Carbon Black
 3MgO
 6Ca(OH)2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin DAI-EL® G-101 Fluoroelastomer Plasticizer with DAI-EL® G-702 Fluoroelastomer
Vicone High Performance Rubber VicoFluor™ 57FK-GR High Performance Fluoroelastomer Rubber
Daikin DAI-EL® G-557 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content
Daikin DAI-EL® G-101 Fluoroelastomer Plasticizer with DAI-EL® G-701 Fluoroelastomer
Chemours Viton® A-HV Fluoroelastomer (FKM)

PDAIJ9951 / 210024

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.