MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elmet-Starck Molybdenum Alloy PBT, Bar
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal

Material Notes: Powder Metallurgy Bar

Description of Product: This specification covers molybdenum alloy (Molybdenum + 0.5% titanium + 0.1% zirconium) wrought bar produced from pressed and sintered powder metallurgy billet.

Structure: Bars can be supplied in the recrystallized condition.

Information provided by H.C. Starck.

Elmet Technologies Acquired H.C. Starck Solutions Americas in 2023.

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers <= 215
@Load 10.0 kg
<= 215
@Load 22.0 lb
mid-radius, recrystallized bar, all sizes; DPH (10 kg)
 230 - 285
@Load 10.0 kg,
Diameter 73.03 - 88.9 mm
230 - 285
@Load 22.0 lb,
Diameter 2.875 - 3.50 in
mid-radius; DPH (10 kg)
 235 - 290
@Load 10.0 kg,
Diameter 47.63 - 73.03 mm
235 - 290
@Load 22.0 lb,
Diameter 1.875 - 2.875 in
mid-radius; DPH (10 kg)
 240 - 300
@Load 10.0 kg,
Diameter 28.57 - 47.63 mm
240 - 300
@Load 22.0 lb,
Diameter 1.125 - 1.875 in
mid-radius; DPH (10 kg)
 245 - 310
@Load 10.0 kg,
Diameter 22.2 - 28.57 mm
245 - 310
@Load 22.0 lb,
Diameter 0.875 - 1.125 in
mid-radius; DPH (10 kg)
 255 - 320
@Load 10.0 kg,
Diameter 3.17 - 22.2 mm
255 - 320
@Load 22.0 lb,
Diameter 0.125 - 0.875 in
mid-radius; DPH (10 kg)
Tensile Strength  >= 586 MPa
@Diameter 73.03 - 88.9 mm
>= 85000 psi
@Diameter 2.875 - 3.50 in
ASTM E-8
 >= 621 MPa
@Diameter 47.63 - 73.03 mm
>= 90000 psi
@Diameter 1.875 - 2.875 in
ASTM E-8
 >= 689 MPa
@Diameter 28.57 - 47.63 mm
>= 100000 psi
@Diameter 1.125 - 1.875 in
ASTM E-8
 >= 758 MPa
@Diameter 22.2 - 28.57 mm
>= 110000 psi
@Diameter 0.875 - 1.125 in
ASTM E-8
 >= 793 MPa
@Diameter 3.17 - 22.2 mm
>= 115000 psi
@Diameter 0.125 - 0.875 in
ASTM E-8
Tensile Strength, Yield  >= 517 MPa
@Diameter 73.03 - 88.9 mm,
Strain 0.2 %
>= 75000 psi
@Diameter 2.875 - 3.50 in,
Strain 0.2 %
ASTM E-8
 >= 552 MPa
@Diameter 47.63 - 73.03 mm,
Strain 0.2 %
>= 80000 psi
@Diameter 1.875 - 2.875 in,
Strain 0.2 %
ASTM E-8
 >= 586 MPa
@Diameter 28.57 - 47.63 mm,
Strain 0.2 %
>= 85000 psi
@Diameter 1.125 - 1.875 in,
Strain 0.2 %
ASTM E-8
 >= 655 MPa
@Diameter 22.2 - 28.57 mm,
Strain 0.2 %
>= 95000 psi
@Diameter 0.875 - 1.125 in,
Strain 0.2 %
ASTM E-8
 >= 689 MPa
@Diameter 3.17 - 22.2 mm,
Strain 0.2 %
>= 100000 psi
@Diameter 0.125 - 0.875 in,
Strain 0.2 %
ASTM E-8
Elongation at Break  >= 5.0 %
@Diameter 73.03 - 88.9 mm
>= 5.0 %
@Diameter 2.875 - 3.50 in
ASTM E-8
 >= 10 %
@Diameter 28.57 - 47.63 mm
>= 10 %
@Diameter 1.125 - 1.875 in
ASTM E-8
 >= 10 %
@Diameter 47.63 - 73.03 mm
>= 10 %
@Diameter 1.875 - 2.875 in
ASTM E-8
 >= 15 %
@Diameter 22.2 - 28.57 mm
>= 15 %
@Diameter 0.875 - 1.125 in
ASTM E-8
 >= 18 %
@Diameter 3.17 - 22.2 mm
>= 18 %
@Diameter 0.125 - 0.875 in
ASTM E-8
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.010 - 0.040 %0.010 - 0.040 %
Iron, Fe <= 0.010 %<= 0.010 %
Molybdenum, Mo >= 99.2 %>= 99.2 %by difference
Nickel, Ni <= 0.0050 %<= 0.0050 %
Nitrogen, N <= 0.0020 %<= 0.0020 %Sintered material
Oxygen, O <= 0.040 %<= 0.040 %Sintered material
Silicon, Si <= 0.0050 %<= 0.0050 %
Titanium, Ti 0.40 - 0.55 %0.40 - 0.55 %
Zirconium, Zr 0.060 - 0.12 %0.060 - 0.12 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
Overview of materials for Molybdenum Alloy
A. Schulman ComAlloy Comtuf® 420 Polyester - PBT, High Impact Modified

NHCST907 / 130797

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.