MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem CP 743 HECO Polypropylene Heterophasic Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: CP 743 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and a general purpose additive package. CP 743 presents high melt strength, good processability, and excellent impact strength. It is designed for thermoforming and extrusion processing. Its applications include: thermoformed packages with high impact strength, sheet extrusion, and compounds.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.895 g/cc0.0323 lb/in³ASTM-D792
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.60 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 5757ASTM-D785
Tensile Strength, Yield 25.0 MPa3630 psiASTM-D638
Elongation at Yield 15 %15 %ASTM-D638
Flexural Modulus, 1% Secant 1000 MPa145000 psiASTM-D790
Izod Impact, Notched  0.370 J/cm
@Temperature -20.0 °C
0.693 ft-lb/in
@Temperature -4.00 °F
ASTM-D256
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM-D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FASTM-D648
Vicat Softening Point 146 °C
@Load 1.02 kg
295 °F
@Load 2.25 lb
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem PRA 0852 RACO Random Polypropylene Copolymer
Braskem Prisma 3410 RACO Random Polypropylene Copolymer
Braskem PRB 0131 RACO Random Polypropylene Copolymer
Braskem Prisma 2400 RACO Random Polypropylene Copolymer
Braskem Prisma 2910 RACO Random Polypropylene Copolymer

PBRAS937 / 106783

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.