MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polycasa Acryl® G 87 E Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Grade for extruding semi-finished products such as twin-strapped panels, profile and tubes, as well as injection molding of watch glasses, dishes, bowls, water-tap hand grips and bathroom fittings, soap dishes, shelves, containers and beakers.

Data was collected by ISO methods.

Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³
Moisture Absorption at Equilibrium 0.30 %0.30 %
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in
Melt Flow 1.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.5 g/10 min
@Load 8.38 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 72.0 MPa10400 psi
Elongation at Break 4.5 %4.5 %
Tensile Modulus 3.20 GPa464 ksi
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
 3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
Dielectric Strength 60.0 kV/mm1520 kV/in
Dissipation Factor  0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
 0.040
@Frequency 100 Hz
0.040
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °F
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °F
Vicat Softening Point 103 °C217 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Oxygen Index 18 %18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® HI-1001B PC/ABS, Unreinforced
Overview of materials for Acrylic, General Purpose, Molded
Eastman Eastar 6763 PETG Copolyester
Lotte Advanced Materials Infino® HI-1001BG PC/ABS, Metal Plating Grade
Mitsubishi Xantar® 24 R Polycarbonate

PSF015 / 66573

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.