MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poraver 0.25-0.5 mm Expanded Glass
Categories: Ceramic; Glass

Material Notes:

Information provided by Poraver®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.288 - 0.391 g/cc0.0104 - 0.0141 lb/in³Dry loose; ASTM C9/C29M
Density 0.591 - 0.771 g/cc0.0214 - 0.0278 lb/in³ASTM C128
Water Absorption 15 %15 %by volume; ASTM C128
 28 %28 %by mass; ASTM C128
Water Absorption at Saturation <= 0.50 %<= 0.50 %
Particle Mesh Size 35 - 60 Mesh35 - 60 MeshASTM C136
pH 9.0 - 129.0 - 12
Thickness 250 - 500 microns9.84 - 19.7 milGrain size; ASTM C136
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 2.60 MPa377 psiEN 13055-1
 
Thermal PropertiesMetricEnglishComments
Softening Point 700 °C1290 °F
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 1.0 %1.0 %ASTM C114
 
Descriptive Properties
Colorcreamy white
Finess Modulus1.92ASTM C136

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Poraver Metapor®
Poraver 1-2 mm Expanded Glass
Poraver 0.1-0.3 mm Expanded Glass
Pyrotek ISOMAG® 175 Structural Insulation Board
Pyrotek NAD-250 Structural Insulation Board

CPOR020 / 186909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.