MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo EMERGE™ 4310-6 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: EMERGE™ PC 4310-6 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. This resin is available in a full range of colors that can be custom tailored to meet your product requirements.

Applications:
  • Consumer Electronics and Information Technology Equipment
  • Computer and Business Equipment
  • Portable Electronics

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Ultimate 72.4 MPa10500 psi0.125 in, injection molded, unannealed; ASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi0.125 in, injection molded, unannealed; ASTM D638
Elongation at Break 150 %150 %0.125 in, injection molded, unannealed; ASTM D638
Tensile Modulus 2.41 GPa350 ksi0.125 in, injection molded, unannealed; ASTM D638
Flexural Strength 96.5 MPa14000 psi0.125 in, injection molded, unannealed; ASTM D790
Flexural Modulus 2.41 GPa350 ksi0.125 in, injection molded, unannealed; ASTM D790
Izod Impact, Notched 9.08 J/cm17.0 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D256
Dart Drop, Total Energy 90.0 J66.4 ft-lb8000 ipm; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+17 ohm-cm2.00e+17 ohm-cmASTM D257
Dielectric Constant  3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.5 kV/mm420 kV/inASTM D149
Dissipation Factor  0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.4 µm/m-°C
@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °F0.157 in, annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C265 °F0.157 in, unannealed; ASTM D648
 142 °C288 °F0.157 in, annealed; ASTM D648
Vicat Softening Point 151 °C304 °F50°C/hr, 50N; ASTM D1525
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in
Oxygen Index 26 %26 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo EMERGE™ 4310-22 Polycarbonate
Trinseo EMERGE™ 4310-15 Polycarbonate
Trinseo EMERGE™ 4310-10 Polycarbonate

PZZDOW1343 / 30561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.