MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Struktol STRUKSILON 8007 Silicone Stabilizer for PU-Rigid Foam
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: STRUKSILON 8007 was developed as universal silicone stabilizer for production of polyurethane rigid foam based on polyester and polyether polyols.

Applications: STRUKSILON 8007 is applicable in combination with the usual blowing agents in systems for nearly all known PU rigid foam applications, e.g. sandwich elements (CLBS), insulation material for production of cooling and heating appliances and facilities, roof and wall insulations in the construction industry and for systems in the block foam area.

Information provided by Struktol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³
Viscosity 900 cP
@Temperature 25.0 °C
900 cP
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 100 °C>= 212 °FDIN/ISO 2562
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.45151.4515
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 12.0 Month>= 12.0 Monthin closed original containers if transported and stored at temperatures between 1 and 30°C
 
Descriptive Properties
AppearanceClear, colorless to slightly yellow liquid
Turbidity Point °C31

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Struktol STRUKSILON 8002 Silicone Stabilizer for PU-Rigid Foam
Struktol STRUKSILON 8104 Silicone Stabilizer for PU Foam
Struktol STRUKSILON 8026 Silicone Stabilizer for PU Foam
Struktol STRUKSILON 8005 Silicone Stabilizer for PU-Rigid Foam
Struktol STRUKSILON 8120 Silicone Stabilizer for PU Foam

PSTRUK69 / 69296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.