A. Schulman BMC 1608 Very High Strength, Corrosion Resistant
Categories:
Polymer
;
Thermoset
;
Polyester, TS
Material Notes:
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was formerly known as Glastic® 1608.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.75
-
1.80
g/cc
1.75
-
1.80
g/cc
Water Absorption
0.12 - 0.20 %
0.12 - 0.20 %
24 hours, 23°C
Linear Mold Shrinkage
0.0010
-
0.0030
cm/cm
0.0010
-
0.0030
in/in
Mechanical Properties
Metric
English
Comments
Hardness, Barcol
40 - 50
40 - 50
Tensile Strength, Ultimate
34.5
-
41.4
MPa
5000
-
6000
psi
Flexural Strength
193
-
200
MPa
28000
-
29000
psi
Flexural Modulus
13.8
-
15.2
GPa
2000
-
2200
ksi
Compressive Strength
234
-
241
MPa
34000
-
35000
psi
Izod Impact, Notched
4.81
-
5.34
J/cm
9.00
-
10.0
ft-lb/in
Electrical Properties
Metric
English
Comments
Dielectric Strength
17.6
kV/mm
447
kV/in
Short Time
Dissipation Factor
0.0050
@Frequency 60 Hz
0.0050
@Frequency 60 Hz
Condition A
0.0080
@Frequency 60 Hz
0.0080
@Frequency 60 Hz
Condition A
0.026
@Frequency 60 Hz
0.026
@Frequency 60 Hz
Condition D
0.115
@Frequency 60 Hz
0.115
@Frequency 60 Hz
Condition D
Arc Resistance
104
sec
104
sec
Track Resistance
1.75
sec
1.75
sec
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
>=
260
°C
>=
500
°F
Flammability, UL94
HB
HB
Processing Properties
Metric
English
Comments
Mold Temperature
138
-
166
°C
280
-
330
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
A. Schulman BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 6241 Glass Fiber Reinforced Compound
A. Schulman BMC 695 Vinyl Ester Molding Compound
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30
PBMC053 / 27236
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.