MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 1022 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Used in cold heading and extruding. Applications include low-strength fasteners, die pins, motor spindles, and recessed-head screws.

Key Words: UNS G10220, AMS 5070, ASTM A29, ASTM A510, ASTM A519, ASTM A544, ASTM A545, ASTM A548, ASTM A576, MIL SPEC MIL-S-11310 (CS1022), SAE J403, SAE J412, SAE J414, DIN 1.1133, UNI G 22 Mn 3, JIS SMnC 21
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.858 g/cc0.2839 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 121121
Hardness, Knoop 140140Converted from Brinell
Hardness, Rockwell B 6868Converted from Brinell
Hardness, Vickers 126126Converted from Brinell
Tensile Strength, Ultimate 425 MPa61600 psi
Tensile Strength, Yield 235 MPa34100 psi
Elongation at Break 23 %23 %in 50 mm
Reduction of Area 47 %47 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000159 ohm-cm
@Temperature 0.000 °C
0.0000159 ohm-cm
@Temperature 32.0 °F
annealed specimen
 0.0000219 ohm-cm
@Temperature 100 °C
0.0000219 ohm-cm
@Temperature 212 °F
annealed specimen
 0.0000293 ohm-cm
@Temperature 200 °C
0.0000293 ohm-cm
@Temperature 392 °F
annealed specimen
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 °C
6.39 µin/in-°F
@Temperature 68.0 °F
Typical steel
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
6.78 µin/in-°F
@Temperature 32.0 - 572 °F
Typical for steel
 13.9 µm/m-°C
@Temperature 0.000 - 500 °C
7.72 µin/in-°F
@Temperature 32.0 - 932 °F
Typical for steel
Specific Heat Capacity 0.472 J/g-°C0.113 BTU/lb-°FTypical steel
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.17 - 0.23 %0.17 - 0.23 %
Iron, Fe 98.68 - 99.13 %98.68 - 99.13 %As remainder
Manganese, Mn 0.70 - 1.0 %0.70 - 1.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1022 Steel, cold drawn round (19 - 32 mm)
AISI 1022 Steel, as rolled
AISI 1018 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1022 Steel, normalized at 925°C (1700°F)
AISI 1021 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round

M1022E / 6856

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.