MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay L-705 Impact Resistant Aramid Prepreg
Categories: Polymer; Thermoset

Material Notes: Description: Designers use L-705 to create laminates capable of withstanding ballistic threats. L-705 is available in a variety of fabric styles to match the engineering requirements for a particular application. The cure cycle for L-705 allows easy processing in a press, oven, or autoclave.

Advantages:

  • L-705 can be used in a stand alone configuration or can be combined with various other engineered materials to create effective ballistic protection from many different threats
  • L-705 is comparable with L-314 adhesive film for bonding to ceramic or steel layers used to prevent penetration of high velocity rounds

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 90.0 min
@Temperature 135 °C
1.00 - 1.50 hour
@Temperature 275 °F
 90.0 - 120 min
@Temperature 121 °C
1.50 - 2.00 hour
@Temperature 250 °F
Shelf Life  1.50 Month
@Temperature 21.0 °C
1.50 Month
@Temperature 69.8 °F
 6.00 Month
@Temperature 4.00 °C
6.00 Month
@Temperature 39.2 °F
 
Descriptive Properties
ColorReddish Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, Aramid Balanced fabric 175 g/m2
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Hexcel® HexForce™ 328 Aramid Fabric
Geon® Performance Solutions 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)
Garlock 3205 Neoprene/Polyester Fabric

PCYTED125 / 180427

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.