MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Covestro Desmodur® MS-092 + Baytec XL B/Baytec XL HQEE, 50D Polyurethane, MDI- Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characteristics:
Properties:
  • Excellent wear and tear resistance
  • Superior tensile strength & elongation
  • Good solvent resistance
  • Low compression set
Comments:
  • Suitable for forklift tires, sheet goods, wheels, & rollers
  • Suitable for sprocket wheels & die-cut pads
  • Ideal for gaskets & seals
  • Excellent general purpose elastomer
  • Improved temperature resistance with HQEE

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccDesmodur MS-092
Viscosity 8.0 cP8.0 cPBaytec XL B
 365 cP365 cPDesmodur MS-092
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050ASTM D412
Tensile Strength at Break 42.1 MPa6110 psiASTM D412
Elongation at Break 480 %480 %ASTM D412
100% Modulus 13.1 MPa
@Strain 100 %
1900 psi
@Strain 100 %
ASTM D412
200% Modulus 15.5 MPa
@Strain 200 %
2250 psi
@Strain 200 %
ASTM D412
300% Modulus 19.3 MPa
@Strain 300 %
2800 psi
@Strain 300 %
ASTM D412
Resilience 4242[%], Bayshore; ASTM D2632
Tear Strength 48.2 kN/m275 pliDie C; ASTM D624
 65.7 kN/m375 pliSplit; ASTM D1938
Taber Abrasion, mg/1000 Cycles 42
@Load 1.00 kg
42
@Load 2.20 lb
H-18 wheel; ASTM D4060
Compression Set 26 %
@Temperature 70.0 °C,
Time 79200 sec
26 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395-B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 50.0 - 70.0 °C122 - 158 °FBaytec XL B
 80.0 - 95.0 °C176 - 203 °FDesmodur MS-092
 100 - 110 °C212 - 230 °FBaytec XL HQEE
Mold Temperature 100 - 110 °C212 - 230 °F
Pot Life 2.00 - 4.00 min2.00 - 4.00 min
 
Descriptive Properties
Appearanceclear liquidBaytec XL B
 tan solidBaytec XL HQEE
 yellow liquidDesmodur MS-092
Content100Parts by weight of Desmodur MS-092 prepolymer*
 19.61Parts by weight of Baytec XL HQEE*
 45 EWNCO, Baytec XL B
 8.95-9.74%NCO, Desmodur MS-092
 99 EWNCO, Baytec XL HQEE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer
Mearthane Durethane™ C 50D Polyurethane
Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D
Mearthane Durethane™ S DS-560D Solid Polyurethane Elastomer
Covestro Desmopan® 9392AU Polyurethane

PCOVEST0503 / 202286

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.