MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon® ETP H4837 High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Applications
ALATHON H 4837 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processability and thermal stability, with good color and organoleptic properties. Typical applications are rigid food containers such as 4, 5, and 6-quart ice cream containers, which are produced at high speeds in fast cycling multi-cavity stack molds.

Regulatory Status
H 4837 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing H 4837 can only be made when the processing conditions, equipment and end use application are known. However, melt temperatures from 475°F to 535°F are recommended for initial start-ups.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.946 g/cc0.0342 lb/in³ASTM D1505
Melt Flow 40 g/10 min40 g/10 minASTM D1238
Spiral Flow 46.7 cm18.4 inSpiral channel (0.625” insert) with injection pressure of 1000 psi at 440°F.; Equistar
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ASTM D2240
Tensile Strength at Break 22.1 MPa3200 psiASTM D638
Tensile Strength, Yield 25.0 MPa3630 psiCrosshead speed - 2"min.; ASTM D638
Elongation at Yield 7.9 %7.9 %Crosshead speed - 2" min; ASTM D638
Flexural Modulus, 1% Secant 979 MPa142000 psiCrosshead speed - 0.5" min; ASTM D790
2% Secant Modulus 0.862 GPa125 ksiCrosshead speed - 0.5" min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 64.0 °C147 °FASTM D648
Vicat Softening Point 121 °C250 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Alathon® ETP H4745 High Density Polyethylene
NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin
LyondellBasell Alathon® ETP H5057 High Density Polyethylene
LyondellBasell Alathon® H5520 High Density Polyethylene

PEQU0121 / 36550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.