MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

H.C. Starck Ni-SA U700 Nickel Super Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Ni-SA (Nickel Super Alloys) prevents high temperature corrosion, pitting and crevice corrosion and oxidation for chemical processings with high mechanical stresses, heat exchanger, gas turbine and engine components, rotor blades, pumps and hot working tools.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 4.15 %<= 4.15 %
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 14 - 16 %14 - 16 %
Cobalt, Co 16 - 18 %16 - 18 %
Molybdenum, Mo 4.5 - 5.5 %4.5 - 5.5 %
Nickel, Ni 52.67 - 65.5 %52.67 - 65.5 %
Titanium, Ti <= 3.65 %<= 3.65 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals UdimetĀ® 700 Nickel Alloy
H.C. Starck Ni-SA 939 Nickel Super Alloy
UnitempĀ® AF2-IDA Nickel Alloy
Special Metals NIMONICĀ® Alloy 105
Tantalum, UNS R05200

NHCSTA016 / 17218

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.