MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexWeb® HRH-36 - 3/16 - 2.0 Para-Aramid/Phenolic Core  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Aramid; Phenolic

Material Notes: Designation: Material-Cell Size (inches)-Density
HexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.

Features: Mechanical properties equivalent to KOREX®; Low moisture pickup; Excellent thermal stability; Smooth cell wall finish.
Applications: HexWeb® HRH-36 is a high performance non-metallic core, available in a wide range of densities, suitable for most composite sandwich applications. It can be readily heat formed to help produce complex components and offers similar mechanical properties to KOREX® core as well as comparable moisture pickup. In addition, HexWeb® HRH-36 offers a weight reduction over higher density NOMEX® honeycomb cores.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0320 g/cc0.00116 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength 0.965 MPa140 psiBare
 1.10 MPa160 psiStabilized
Shear Modulus 0.0338 GPa4.90 ksiPlate Shear, W Direction
 0.0689 GPa10.0 ksiPlate Shear, L Direction
Shear Strength 0.483 MPa70.0 psiPlate Shear, W Direction
 0.827 MPa120 psiPlate Shear, L Direction

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRH-36 - 1/8 - 2.5 Para-Aramid/Phenolic Core
Hexcel® HexWeb® HDC-660 - 3/16 - 17.5 (R2) Heavy Density Core
Hexcel® HexWeb® HRH-36 - 1/8 - 4.0 Para-Aramid/Phenolic Core
Hexcel® HexWeb® HRH-10 - 3/16 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
Hexcel® HexWeb® HDC - 3/16 - 16.0 (R2) Heavy Density Core

PHEXC361 / 98832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.