MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toho Tenax Pyromex® CPX 2d 312K Non-crimped Carbon Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Pyromex® is an oxidized organic polyacrylonitrile (PAN) fiber with excellent heat and flame resistance. It also features excellent resistance to chemicals and good electrical insulation properties. In addition, unlike inorganic fibers, this yarn is highly processable for yarn spinning and weaving. Pyromex® is widely used in anti-spattering sheets for welding, fleeces or needle felts for heat protection in the auto or aerospace industries, heat protective clothing, protective covering for furnaces, heat insulators, brake or clutch discs, and high temperature carbon/carbon composite (C/C) parts. It is available as tow or staple fiber. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³
Water Absorption at Saturation 7.0 %7.0 %Typical Moisture Content
Fiber Count 2.20 dtex1.98 denierIndividual Filament
 686000 dtex617000 denierTow Yield, Dry
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 20 %20 %Dry
Tenacity 0.203 N/tex2.30 g/denierDry
 
Descriptive Properties
Finish0.5%
Number of Filaments312000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DowAksa AKSACA™ A-49 D 24K Continuous Carbon Fiber
Toho Tenax Pyromex® PX 2d Crimped Carbon Fiber
AISI 4028 Steel
AISI 4032 Steel, Annealed Cold Drawn Bar
Beijing Evergrow Resources Carbon Fiber Felt

ETOHO56 / 6130

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.