MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Fusabond® C190 Polymer Modifier
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DuPont™ Fusabond® C190 is a anhydride modified ethylene vinyl acetate copolymer.

Uses:

  • Adhesives
  • Pipe Coating
  • Polymer Modifier

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792, ISO 1183
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 190 °C
16 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 71.0 °C160 °FASTM D3418, ISO 3146
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 260 °C<= 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Fusabond® N416 Polymer Modifier
Dow Fusabond® C250 Polymer Modifier
Dow Fusabond® A560 Polymer Modifier
Dow Fusabond® E158 Polymer Modifier
Dow Fusabond® E265 Polymer Modifier

PDTA4964 / 170404

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.