MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Titanium Ti-7Al-4Mo Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Annealed 790ºC. Alpha-Beta Alloy. High strength. Good creep resistance.

Applications: Aerospace, jet engine disks, compressor blades and spacers, sonic horns

1 other heat treatment of this alloy is in MatWeb.

Key Words: UNS R56740
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.48 g/cc0.162 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 318318Estimated from Rockwell C.
Hardness, Knoop 346346Estimated from Rockwell C.
Hardness, Rockwell C 3434
Hardness, Vickers 333333Estimated from Rockwell C.
Tensile Strength, Ultimate 1030 MPa149000 psi
Tensile Strength, Yield 970 MPa141000 psi
Tensile Modulus 111 GPa16100 ksi
Compressive Modulus 111 GPa16100 ksi
Poissons Ratio 0.320.32
Shear Modulus 42.0 GPa6090 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000170 ohm-cm0.000170 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.00 µm/m-°C
@Temperature 20.0 - 100 °C
5.00 µin/in-°F
@Temperature 68.0 - 212 °F
 9.40 µm/m-°C
@Temperature 20.0 - 315 °C
5.22 µin/in-°F
@Temperature 68.0 - 599 °F
average
 10.4 µm/m-°C
@Temperature 20.0 - 615 °C
5.78 µin/in-°F
@Temperature 68.0 - 1140 °F
average
Specific Heat Capacity 0.515 J/g-°C0.123 BTU/lb-°F
Thermal Conductivity 6.10 W/m-K42.3 BTU-in/hr-ft²-°F
 10.4 W/m-K
@Temperature 315 °C
72.2 BTU-in/hr-ft²-°F
@Temperature 599 °F
 12.1 W/m-K
@Temperature 427 °C
84.0 BTU-in/hr-ft²-°F
@Temperature 801 °F
 13.8 W/m-K
@Temperature 540 °C
95.8 BTU-in/hr-ft²-°F
@Temperature 1000 °F
Melting Point <= 1650 °C<= 3000 °F
Liquidus 1650 °C3000 °F
Maximum Service Temperature, Air 480 °C896 °F
Beta Transus 1005 °C1841 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 7.0 %7.0 %
Carbon, C <= 0.10 %<= 0.10 %
Hydrogen, H <= 0.013 %<= 0.013 %
Iron, Fe <= 0.30 %<= 0.30 %
Molybdenum, Mo 4.0 %4.0 %
Nitrogen, N <= 0.050 %<= 0.050 %
Oxygen, O <= 0.20 %<= 0.20 %
Titanium, Ti 89 %89 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-7Al-4Mo, STA
Titanium Ti-6Al-4V (Grade 5), Annealed Bar
Titanium Ti-6Al-6V-2Sn (Ti-6-6-2) Annealed
Titanium Ti-5Al-6Sn-2Zr-1Mo-0.25Si
Titanium Ti-6Al-4V (Grade 5), STA Bar

MTP742 / 14248

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.