MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Polylac® PA766 ABS Resin - Flame Retardant Grade  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Medium Impact, Octa-Deca Grade

Typical properties; not to be construed as specifications. Mechanical properties measured on 1/8 in. Type I specimens.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
Melt Flow  2.3 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.3 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
25 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO-1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ASTM D785
Tensile Strength, Yield 37.2 MPa5400 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Tensile Modulus 2.48 GPa360 ksiASTM D638
Flexural Yield Strength 57.7 MPa8370 psiASTM D790
Flexural Modulus 1.93 GPa280 ksiASTM D790
Izod Impact, Notched  2.16 J/cm
@Thickness 6.35 mm
4.05 ft-lb/in
@Thickness 0.250 in
ASTM D256
 2.38 J/cm
@Thickness 3.17 mm
4.46 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °F1/8 in, Unannealed; ASTM D648
 88.0 °C190 °F1/8 in, Annealed; ASTM D648
Vicat Softening Point 101 °C214 °FASTM D1525
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-737 ABS - High Flow
Chi Mei Polylac® PA-763 ABS - Flame Retardant
Chi Mei Polylac® PA-763A ABS - Flame Retardant
Chi Mei Polylac® PA-764 ABS - Flame Retardant
Chi Mei Polylac® PA-764B ABS - Flame Retardant

PLBZ50 / 50523

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.